Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Carburized Layer and Decarburized Layer Depth Testing

Carburized layer and decarburized layer depth testing is a critical metallurgical evaluation that measures the hardened case depth and surface carbon loss of steel components after heat treatment, hot rolling, or forging. Accurate determination of case depth and decarburization depth directly affects wear resistance, fatigue performance, and machinability, making it essential for quality control in the automotive, aerospace, bearing, and fastener industries. Accredited third-party laboratories perform these tests in accordance with international standards such as ISO 2639, ISO 3887, ASTM E1077, GB/T 9450, and GB/T 224.

Technical Overview

Carburizing is a case-hardening heat treatment in which carbon is diffused into the surface of a low-carbon steel at elevated temperature, followed by quenching and tempering to produce a hard, wear-resistant surface over a tough core. The performance of a carburized component is governed by its case depth, which is classified into effective case depth, defined as the distance from the surface to the point where hardness reaches a specified hardness limit (commonly 550 HV1 or approximately 52 HRC), and total case depth, defined as the distance from the surface to the point where the microstructure is no longer distinguishable from the core structure.

Decarburization is the opposite phenomenon: the loss of surface carbon that occurs when steel is heated in an oxidizing or poorly controlled furnace atmosphere during rolling, forging, annealing, or heat treatment. Decarburization is categorized into complete decarburization, where the surface is fully transformed to ferrite, and partial decarburization, where the carbon content is reduced but the structure is not fully ferritic. The total decarburized depth is the sum of both zones. A decarburized surface exhibits reduced hardness, poor fatigue strength, soft spots after quenching, and an elevated risk of premature crack initiation.

Both parameters must be quantified precisely because under-sized carburized cases lead to surface spalling, pitting, and rapid wear, while excessive decarburization compromises surface integrity and fatigue life. Accredited third-party laboratories conduct these measurements using microhardness profiling and quantitative metallography in accordance with ISO 2639, ISO 3887, ASTM E1077, GB/T 9450, GB/T 9451, GB/T 224, EN standards, and JIS G 0558/G 0559, providing traceable, decision-grade data for product release and process validation.

Testing Samples

Carburized and Carbonitrided Components

Typical samples include transmission gears, camshafts, crankshafts, CV joints, splined shafts, bushings, pins, clutch components, and other dynamically loaded parts that require a hard case over a ductile core. Samples may be submitted as finished parts, heat-treated blanks, or witness coupons processed alongside production loads.

Decarburization-Sensitive Products

Samples such as spring steel wire and strip, hot-rolled and forged bars, oil-tempered wire, fastener rod, cold-heading wire, rails, and stamped components are routinely evaluated for surface carbon loss, because even a shallow decarburized layer can drastically reduce fatigue performance in these products.

Raw Materials and In-Process Specimens

Steel mills, forgers, and heat-treatment suppliers submit billet slices, rolled rod sections, ring-rolled bearing races, and furnace trial coupons to verify atmosphere control and to certify compliance with purchase specifications before downstream processing.

Testing Items

The core measurable parameters for this testing service include:

  • Effective case depth (CHD) determined by hardness limit, typically 550 HV1
  • Total case depth determined by microstructural transition
  • Surface hardness, intermediate hardness profile, and core hardness
  • Total decarburized depth, including both complete and partial zones
  • Complete decarburization depth, measured as the surface ferrite rim
  • Partial decarburization depth, measured from the end of the ferrite zone to the unaffected base structure
  • Effective or ferritic decarburization depth where specified by the product standard
  • Carbon concentration profile as a function of depth
  • Supporting microstructure evaluation, including carbide networks, retained austenite, internal oxidation, and grain-boundary oxidation depth

Testing Methods

Microhardness Traverse Method for Case Depth

In accordance with GB/T 9450, ISO 2639, and SAE J423, a polished transverse section is subjected to a series of Vickers indentations (HV0.5 or HV1) starting approximately 0.05 mm below the surface and continuing at intervals not exceeding 0.1 mm. Indentation diagonals are limited so that they do not overlap or interact with the specimen edge. The effective case depth is the distance from the surface to the location where hardness falls to the specified limit, often 550 HV1 for carburized case-hardening steels. For very thin hardened layers below 0.3 mm, the procedures of GB/T 9451 are applied with appropriately reduced test forces.

Metallographic Method for Case Depth

A full cross-section is mounted, ground, and polished to a finish of 1 micron or better, then etched with 2 to 4 percent nital. The total case depth is measured under an optical microscope at suitable magnification as the distance from the surface to the point where the microstructure becomes indistinguishable from the core, based on the transition from hypereutectoid and eutectoid constituents to the hypoeutectoid core structure.

Metallographic Method for Decarburization Depth

Following GB/T 224, ISO 3887, ASTM E1077, and JIS G 0559, the polished and nital-etched cross-section is examined to measure the complete decarburization zone, characterized by a fully ferritic surface layer, and the partial decarburization zone, where carbon content is reduced relative to the core. The total decarburized depth is reported as the sum of the two zones, typically as the average and maximum of multiple fields measured around the perimeter.

Microhardness Method for Decarburization Depth

Where the microstructural gradient is ambiguous, for example in quenched and tempered or spheroidize-annealed steels, a Vickers or Knoop hardness profile is taken from the surface inward. The decarburized depth is defined as the depth at which hardness recovers to a specified fraction of the unaffected base-metal hardness, or to the level established by reference to a properly processed companion specimen.

Chemical Analysis Method

For reference-depth determination or dispute resolution, material is removed in thin, controlled increments by precision turning or layer grinding, and the carbon content of each layer is determined by combustion infrared absorption analysis. The decarburized depth corresponds to the layer at which carbon content returns to the specified or nominal base value.

Specimen Preparation and Quality Control

Careful sectioning with abundant coolant, avoidance of grinding burn and tempering of the surface, sharp edge retention during polishing, calibrated microhardness testers verified per ISO 6507 and ASTM E92, and certified reference microscopes ensure that measurements are accurate, repeatable, and traceable.

Applications

Carburized layer and decarburized layer depth testing supports quality assurance, material qualification, and failure investigation across many industries:

  • Automotive: qualification and release of carburized gears, camshafts, differential components, and constant-velocity joints
  • Bearings: verification of hardened depth on races, rollers, and ring-rolled bearing components
  • Fasteners: evaluation of decarburization on high-strength bolt stock and cold-heading wire before and after heat treatment
  • Spring manufacturing: control of decarburized depth on spring steel strip, wire, and oil-tempered products, where fatigue life is directly affected
  • Steel production: certification of hot-rolled bars, rods, and sections against product specification limits
  • Aerospace and wind power: process validation and periodic surveillance of case-hardened actuation, gearing, and turbine drive components
  • Failure analysis: confirmation of whether insufficient case depth or surface decarburization contributed to wear, spalling, or fatigue fracture
  • Heat-treatment suppliers: furnace atmosphere audits, process capability studies, and first-article inspection

FAQ

What is the difference between total case depth and effective case depth?

Total case depth is a metallographic measure extending from the surface to the point where the microstructure no longer differs from the core, whereas effective case depth is a functional, hardness-based measure extending from the surface to the depth at which hardness falls to a defined limit, typically 550 HV1. Effective case depth is normally the acceptance criterion in component specifications.

What is the difference between complete and partial decarburization?

Complete decarburization produces a fully ferritic surface layer in which carbon has been essentially removed, while partial decarburization is a transition zone in which carbon content is lower than the core but the structure is not fully ferritic. The total decarburized depth is the sum of both regions, and many specifications also impose a separate, tighter limit on the complete decarburization depth.

Which standards govern these tests?

Case depth testing is commonly performed to GB/T 9450, GB/T 9451, ISO 2639, and SAE J423, while decarburization depth testing follows GB/T 224, ISO 3887, ASTM E1077, and JIS G 0559. The applicable standard is selected based on the product drawing, purchase specification, or agreement between the purchaser and supplier.

How should samples be prepared and submitted?

Samples should be representative of the delivered condition, kept free of additional heat, grinding, or mechanical damage, and ideally submitted as full cross-sections. For finished parts, the critical location, such as a gear tooth flank or a thread root, should be identified so that the measurement plane captures the functionally significant surface.

How are the results reported?

A typical report states the testing standard, specimen orientation, etchant, hardness test force, magnification, individual and average depth values, the maximum and minimum values around the section, supporting hardness profile data or micrographs, and a clear statement of conformity to the specified limits. All results issued by accredited third-party laboratories are traceable to calibrated equipment and certified reference materials.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing