Coal reactivity determination measures the ability of coal or coal char to react with carbon dioxide at elevated temperatures, a key parameter for evaluating feedstocks for gasification, combustion, and metallurgical processes. The test is typically performed in accordance with GB/T 220, which quantifies the degree of CO2 reduction to CO across a temperature range of 800 °C to 1100 °C. This article explains the testing principle, sample requirements, procedures, result interpretation, and practical applications of coal reactivity measurement.
Technical Overview
Coal reactivity refers to the capacity of the carbonaceous matter in coal to react chemically with gaseous agents such as carbon dioxide, oxygen, or steam at high temperature. In industrial practice and standardized testing, coal reactivity is defined as the reactivity of coal char toward carbon dioxide, governed by the endothermic Boudouard reaction:
C + CO2 → 2CO
The higher the reaction rate of the char with CO2, the more reactive the coal is considered to be. Reactivity is fundamentally influenced by coal rank, maceral composition, pore structure and internal surface area, particle size, and the catalytic effects of mineral matter (particularly potassium, sodium, calcium, and iron compounds). In general, low-rank coals such as lignite and sub-bituminous coal exhibit higher reactivity than high-rank anthracite.
The prevailing national standard for this measurement is GB/T 220, which specifies the determination of the chemical reactivity of coal with carbon dioxide. The result is expressed as the degree of CO2 reduction, denoted as α (percent), measured at a series of test temperatures from 800 °C to 1100 °C in 50 °C increments, and the data are commonly presented as a reactivity–temperature (α–T) curve.
Testing Samples
Bituminous Coal and Anthracite
Hard coals of all ranks can be tested. The sample is air-dried, crushed, and sieved to the standard particle size fraction of 3–6 mm. Sufficient sample quantity (typically several hundred grams) should be submitted to allow for carbonization, repeat determinations, and retention.
Lignite and Low-Rank Coal
Low-rank coals are highly reactive and usually show substantial CO2 conversion already at the lower end of the temperature range. Because of their high moisture and volatile matter content, careful air-drying and handling are required before testing.
Coal Char and Carbonized Materials
Prepared char (the solid residue after carbonization) is the actual material reacted in the test. Coal samples are carbonized in the laboratory at approximately 900 °C to drive off volatile matter before the reactivity measurement, ensuring the result reflects the gasification behavior of the fixed carbon.
Metallurgical Coke
For coke, the analogous property is the Coke Reactivity Index (CRI), determined together with Coke Strength after Reaction (CSR) according to GB/T 4000 or ISO 18894. This is a separate but closely related determination frequently requested alongside coal reactivity testing.
Testing Items
Typical test items and reported results for coal reactivity determination include:
- CO2 chemical reactivity α (%) determined at 800 °C, 850 °C, 900 °C, 950 °C, 1000 °C, 1050 °C, and 1100 °C
- The complete reactivity–temperature (α–T) curve
- The temperature at which the CO2 reduction degree α reaches a specified value (for example, 50 %)
- Volume fraction of CO in the outlet gas at each test temperature
- Coke Reactivity Index (CRI) and Coke Strength after Reaction (CSR) for coke samples, per GB/T 4000 / ISO 18894
- Optional kinetic characterization (apparent activation energy and reaction rate constants) by thermogravimetric methods for research purposes
Testing Methods
Standard Method per GB/T 220 (Coal Reactivity to CO2)
The determination is carried out in an electrically heated tubular furnace equipped with a heat- and corrosion-resistant reaction tube, a carbon dioxide supply with flow control, a temperature control and measurement system, and a gas analysis device. The general procedure is as follows:
- Sample preparation: the air-dried coal is crushed and sieved to obtain the 3–6 mm particle size fraction.
- Carbonization: the sized coal is heated at approximately 900 °C in the carbonization furnace to remove volatile matter and produce a uniform char, which is then cooled under protective conditions and re-sieved to 3–6 mm.
- Reaction: a weighed charge of the char is loaded into the reaction tube and heated in the furnace. When the temperature stabilizes at 800 °C, carbon dioxide of the specified purity is passed through the sample at a controlled flow rate of approximately 0.5 L/min.
- Gas analysis: after the gas composition stabilizes, the CO content of the outlet gas is measured using an infrared gas analyzer, gas chromatograph, or chemical absorption gas analyzer.
- Temperature series: the temperature is then raised in 50 °C steps up to 1100 °C, and the measurement is repeated at each plateau.
The degree of CO2 reduction (reactivity) at each temperature is calculated from the measured gas compositions using the following relationship:
α = [100 × b] / [a × (200 − b)] × 100
where a is the volume fraction of CO2 in the feed gas (%) and b is the volume fraction of CO in the outlet gas (%). The α values are tabulated and plotted against temperature, and repeatability limits specified in the standard must be met for the result to be valid.
Coke Reactivity Method (GB/T 4000 / ISO 18894)
For metallurgical coke, a representative sample of about 200 g in the specified size range (approximately 19–22 mm) is reacted with CO2 at 1100 °C for 2 hours. The percentage of mass loss is reported as the Coke Reactivity Index (CRI). The reacted coke is then tumbled in a specified drum, and the percentage of material larger than 10 mm is reported as the Coke Strength after Reaction (CSR).
Thermogravimetric (TGA) Methods
In research and development settings, gasification reactivity is frequently characterized by thermogravimetric analysis, in which a milligram-scale sample is heated under CO2 in isothermal or non-isothermal modes. Conversion–time and conversion–temperature data are used to derive rate parameters and apparent activation energies. TGA results are highly sensitive to experimental conditions and are not directly interchangeable with the standardized GB/T 220 reactivity values.
Applications
Coal reactivity data are used across the coal utilization and metallurgical industries, including:
- Feedstock screening and selection for fixed-bed, fluidized-bed, and entrained-flow gasifiers, where highly reactive coals allow lower operating temperatures and higher conversion efficiency
- Evaluation of pulverized coal for blast furnace injection, since reactivity correlates with burnout behavior in the raceway
- Coke quality assessment and blend design, using CRI/CSR results to predict coke performance in the blast furnace
- Process modeling and furnace design for producer gas plants, lime kilns, cement kilns, and other coal-fired industrial equipment
- Production of activated carbon and other carbon materials, where reactivity governs activation rates and pore development
- Underground coal gasification feasibility studies and catalytic gasification research
- Coal classification, quality control in mining and trading, and due-diligence testing by accredited third-party laboratories
FAQ
What is coal reactivity and why is it important?
Coal reactivity describes how readily the carbon in coal or char reacts with gases such as CO2 at high temperature. It is a critical quality indicator for gasification, combustion, and injection applications because it directly affects reaction rate, conversion efficiency, operating temperature, and equipment sizing.
Which standards govern coal reactivity determination?
Coal reactivity to carbon dioxide is determined according to GB/T 220. For metallurgical coke, the corresponding properties (CRI and CSR) are determined according to GB/T 4000 or ISO 18894. Research-grade gasification reactivity is often measured by thermogravimetric analysis, for which no single international standard applies.
Why is the coal carbonized before the reactivity test?
Carbonization at approximately 900 °C removes volatile matter so that the measured reaction reflects the gasification behavior of the fixed carbon skeleton rather than devolatilization. This produces comparable results across coals of very different volatile matter contents.
What temperature range is used in the test?
The standard test measures the CO2 reduction degree at 50 °C intervals from 800 °C to 1100 °C. Highly reactive coals show significant CO2 conversion at lower temperatures, while unreactive coals may only approach full conversion near 1100 °C.
How should the results be interpreted?
A higher α value at a given temperature indicates a more reactive coal. Users often compare the α–T curves of different coals, or quote the temperature at which α reaches a defined threshold such as 50 %. Selection depends on the process: high reactivity is desirable for gasification and PCI, while moderate reactivity combined with adequate strength is preferred for coking coals.
What sample quantity and turnaround time are required?
A sample of roughly 0.5–1 kg of 3–6 mm coal is generally sufficient for carbonization, the full temperature series, and repeat determinations. Including carbonization, testing, and reporting, a typical turnaround is several working days, depending on the laboratory workload and whether repeat or supplementary tests are required.
Why Choose ZKGX?
- State-of-the-art analytical equipment
- Highly qualified scientific team
- Fast turnaround time
- Competitive pricing