Ubicación: Global + English
Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Corrugated Paper Tensile Strength Testing: Standards, Methods and Applications

Corrugated paper tensile strength determination is a fundamental physical performance test that measures the maximum tensile force a paper strip can withstand before rupture, expressed as force per unit width in kN/m. This guide explains the applicable ISO, ASTM, and GB/T standards, sample requirements, test procedures, calculation methods, and industrial applications for linerboard, corrugating medium, and corrugated board tested by accredited third-party laboratories.

Technical Overview

Tensile strength is one of the most important mechanical properties of corrugated paper materials. During the determination, a strip of paper of specified width is clamped at both ends in a tensile testing machine and stretched at a controlled rate until it breaks. The maximum force recorded at rupture, divided by the width of the specimen, gives the tensile strength, typically reported in kN/m. Because paper is an anisotropic material, the test is performed separately in the machine direction (MD) and the cross direction (CD), and MD values are usually significantly higher than CD values.

For corrugated packaging, tensile strength directly reflects the ability of linerboard and corrugating medium to withstand the tensile stresses imposed during corrugating, printing, die-cutting, and converting operations, as well as the in-service loads carried by box walls. In addition to tensile strength itself, the test yields elongation at break and tensile energy absorption (TEA), which describe the stretchability and toughness of the sheet. Derived indices such as tensile index (N·m/g) and breaking length (km) allow comparison between papers of different grammages and are widely used in supplier specifications and trade contracts.

Testing Samples

Linerboard (Kraft Liner and Test Liner)

Linerboard forms the outer and inner facings of corrugated board. Typical grammages range from approximately 120 g/m² to 440 g/m². Both virgin kraft liner and recycled test liner are tested in MD and CD to verify that the facing layers can resist the tension applied on the corrugator and in subsequent converting steps.

Corrugating Medium (Fluting)

Corrugating medium is the fluted layer between the liners, usually in the range of 90 g/m² to 180 g/m², produced from semi-chemical or recycled fiber. Adequate MD tensile strength and stiffness are essential because the medium is pulled over corrugating rolls under heat and tension, and weak medium leads to flute fracture and board defects.

Finished Corrugated Board and Board Components

For finished single-wall, double-wall, or triple-wall board, the individual paper plies can be separated and tested, or strips cut from the board faces can be evaluated where the test method permits. Structural board properties such as edge crush are covered by separate methods, but tensile data of the components are key inputs for board and box performance modeling.

Other Paper and Paperboard Grades

White top linerboard, bleached grades, specialty packaging papers, and paper samples submitted for research or failure analysis can also be tested under the same tensile determination procedures, provided the specimens can be cut cleanly to the required dimensions.

Testing Items

A complete corrugated paper tensile strength determination typically includes the following measured and calculated parameters:

  • Tensile strength in the machine direction (MD), expressed in kN/m
  • Tensile strength in the cross direction (CD), expressed in kN/m
  • Tensile index (N·m/g), calculated by dividing tensile strength by grammage determined according to ISO 536
  • Breaking length (km), a derived strength parameter independent of grammage
  • Elongation at break (%), indicating the stretch capability of the sheet
  • Tensile energy absorption (TEA, J/m²), representing the work required to rupture the specimen
  • Z-directional tensile strength (internal bond strength) according to ISO 15754, where delamination resistance is of concern
  • Statistical treatment of results, including mean value, standard deviation, and coefficient of variation

Testing Methods

Reference Standards

Tensile testing of corrugated paper materials is performed in accordance with internationally and nationally recognized standards, including ISO 1924-1 (constant rate of loading method), ISO 1924-2 (constant rate of elongation method, 20 mm/min), ISO 1924-3 (constant rate of elongation method, 100 mm/min), ASTM D828 for tensile properties of paper and paperboard using constant-rate-of-elongation apparatus, and GB/T 12914, the Chinese national standard for the determination of tensile properties of paper and board. Conditioning of test pieces is carried out according to ISO 187.

Specimen Preparation

Specimens are cut with a precision cutter to a width of 15.0 mm ± 0.1 mm and a length sufficient for the selected grip separation, commonly a 100 mm test span with a free length of approximately 250 mm. The cutting edges must be clean, parallel, and free of burrs or defects. At least ten valid specimens are prepared for each direction, clearly marked MD or CD, and any strips containing wrinkles, cuts, watermarks, or visible damage are discarded. Test pieces should be handled by their ends only, since contamination of the test span affects the results.

Conditioning

Before testing, specimens are conditioned to equilibrium in the standard atmosphere of 23 °C ± 1 °C and 50% ± 2% relative humidity as specified in ISO 187. Conditioning is essential because paper tensile properties are strongly influenced by moisture content, and comparison of results is only valid when all samples are tested under identical atmospheric conditions.

Test Procedure

The specimen is mounted centrally between the clamps of a calibrated universal tensile testing machine or dedicated paper tensile tester, with the long axis aligned to the direction of applied force. After verifying correct clamping without slippage, the crosshead is driven at the specified rate, for example 20 mm/min in accordance with ISO 1924-2 or 100 mm/min in accordance with ISO 1924-3, until the specimen ruptures. The maximum force and the elongation at break are recorded. Specimens that break within a few millimeters of the jaw faces, or that slip during testing, are rejected as invalid, and additional specimens are tested until at least ten valid results are obtained for each direction.

Calculation and Reporting

Tensile strength is calculated as the maximum force divided by the specimen width. Tensile index is obtained by dividing the tensile strength in N/m by the grammage in g/m², and breaking length is derived from the tensile index. Tensile energy absorption is determined from the area under the force–elongation curve divided by the area of the test span. The test report shall state the test standard used, conditioning atmosphere, machine direction or cross direction, number of specimens, arithmetic mean, maximum and minimum values, standard deviation, test speed, and gauge length, ensuring full traceability of the results.

Applications

Tensile strength data for corrugated paper materials are used throughout the packaging value chain. Box plants rely on incoming inspection tensile testing to verify that purchased linerboard and medium meet contractual specifications before committing them to production. Packaging engineers use MD and CD tensile properties together with grammage, short-span compression, and burst data as inputs for board design and box compression performance prediction. Manufacturers apply the results for supplier qualification, batch release, and long-term quality trend monitoring.

In research and development, tensile determination is used to evaluate the effects of fiber furnish, recycled fiber content, refining intensity, and chemical additives on paper strength. The test also supports certification of transport packaging, including performance-oriented packaging for dangerous goods, where documented material strength evidence is required. In failure analysis, abnormally low tensile strength often identifies moisture damage, fiber degradation, or improper converting conditions as the root cause of box failures in the field.

FAQ

How many specimens are required for one tensile strength determination?

At least ten valid specimens should be tested for each direction (MD and CD). Specimens that break at the jaw line or slip must be discarded and replaced until the required number of valid results is obtained, ensuring statistical reliability of the mean value.

Why are machine direction and cross direction results different?

Paper fibers orient predominantly along the machine direction during sheet forming on the paper machine. As a result, MD tensile strength is typically substantially higher than CD tensile strength, and both directions must be reported to fully characterize the material.

What are typical tensile index values for corrugated papers?

Values vary widely with furnish and grammage, but virgin kraft linerboard commonly reaches tensile indices well above 40 N·m/g in the machine direction, while recycled grades and corrugating medium generally fall in lower ranges. Contractual limits should always be agreed between buyer and supplier based on the intended application.

Can finished corrugated board be tested directly for tensile strength?

Tensile determination is normally performed on the paper components, that is, the liners and the medium. For finished board, structural tests such as edge crush and burst strength are more commonly specified, although component tensile data remain essential inputs for evaluating overall board performance.

How should samples be submitted to an accredited third-party laboratory?

Samples should be protected from moisture, crushing, and edge damage during transport. A sufficient quantity of full sheets or cleanly cut strips should be provided so that at least ten valid specimens per direction can be prepared, and the machine direction should be clearly marked on each sample.

What is the typical turnaround time for a tensile strength test?

Because specimens must be conditioned to equilibrium before testing, most accredited third-party laboratories complete routine tensile determinations within approximately three to seven working days after sample receipt, depending on the scope of testing and the number of directions and parameters requested.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing