Ubicación: Global + English
Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Extractables and Leachables (E&L) Testing Analysis: Standards, Methods, and Applications

Extractables and leachables (E&L) testing analysis is a critical analytical discipline that identifies, quantifies, and evaluates chemical compounds migrating from packaging materials, medical devices, and product-contact components into pharmaceuticals, foods, and consumer products. Guided by internationally recognized standards from USP, ISO, ICH, EN, and GB, E&L studies safeguard patient and consumer safety while supporting regulatory submissions worldwide. This comprehensive technical guide covers sample types, testing items, analytical methods, study workflow, and practical applications of extractables and leachables analysis.

Technical Overview

Extractables and leachables (E&L) testing analysis is a systematic scientific evaluation of chemical substances that can transfer from polymeric, elastomeric, glass, metallic, or coated materials into a contacted product. The discipline is fundamental to quality assurance for pharmaceutical packaging, medical devices, single-use bioprocessing systems, and food contact materials.

Two complementary concepts define the scope of the analysis:

  • Extractables are compounds that can be released from a material under exaggerated laboratory conditions, such as aggressive solvents, elevated temperatures, or extended contact durations. They represent the “worst-case” chemical profile of the material.
  • Leachables are compounds that actually migrate into the drug product, food, or consumer product under normal conditions of manufacture, storage, and use. Leachables are typically a subset of extractables but may also include reaction products formed through interaction with the product matrix.

The regulatory and compendial framework governing E&L studies includes:

  • USP General Chapters <1663> and <1664> for the assessment of extractables and leachables associated with pharmaceutical packaging and delivery systems
  • USP General Chapters <665> and <1665> for plastic components and systems used in pharmaceutical and biopharmaceutical manufacturing
  • ICH Q3E guideline on extractables and leachables, and ICH Q3D for elemental impurities
  • ISO 10993 series (notably ISO 10993-12 for sample preparation, ISO 10993-17 for toxicological risk assessment, and ISO 10993-18 for chemical characterization) for medical devices
  • EU Regulation No. 10/2011 and the EN 1186 series for plastics in food contact, together with the GB 4806 and GB 31604 series for food contact materials in China
  • ASTM extraction and migration test methods for polymeric materials and food contact articles

A key quantitative output of modern E&L studies is the Analytical Evaluation Threshold (AET), derived from the Safety Concern Threshold (SCT), commonly set at 1.5 µg/day for parenteral, inhalation, and oral routes of exposure. All detected extractables and leachables are reported against the AET so that toxicologists can determine whether any compound presents a safety concern.

Testing Samples

Pharmaceutical Packaging and Delivery Systems

Primary packaging components are the most frequently tested sample category, including blister films (PVC, PVDC, COC, COP), glass vials and ampoules, elastomeric closures and stoppers, aluminum crimp seals, pre-filled syringes (barrels, plungers, needle shields), metered-dose inhaler components, dropper bottles, and laminated flexible films for liquid and powder products.

Medical Devices and Biomaterials

Samples include catheters, intravenous infusion sets and cannulae, blood bags and tubing, hemodialysis membranes, syringes, wound dressings, orthopedic and dental implants, resins and adhesives, breathing circuits, and device coatings. Chemical characterization under ISO 10993-18 is typically performed on the final device or representative material coupons.

Single-Use Bioprocessing Systems

Disposable bags, filter membranes and housings, tubing, connectors, valves, sensors, and mixing systems used in upstream and downstream bioprocessing are evaluated for extractables to protect biological drug product quality throughout the manufacturing chain.

Food Contact Materials and Articles

Testing covers plastic films and containers, metal can coatings, paper and board packaging, silicone rubber utensils, baby bottles and teats, kitchen appliances, cookware non-stick coatings, and reusable food service items.

Other Consumer and Regulated Products

Electronic cigarette and vaping devices, e-liquid containers, cosmetics packaging, drinking water contact materials and pipes, and adhesives or inks used in packaging construction are also subject to E&L or migration evaluation.

Testing Items

A comprehensive E&L program typically addresses the following categories of analytes:

  • Volatile organic compounds (VOC): residual solvents such as toluene, benzene, and ethylbenzene; monomers such as styrene, vinyl chloride, acrylonitrile, and 1,3-butadiene
  • Semi-volatile organic compounds (SVOC): plasticizers including phthalates (DEHP, DINP, DBP), citrates, and adipates; hindered phenol and phosphite antioxidants and their degradation products such as 2,4-di-tert-butylphenol; lubricants and slip agents such as oleamide, erucamide, and stearamide; UV stabilizers and benzophenone-type photoinitiators
  • Non-volatile organic compounds (NVOC): oligomers (cyclic siloxanes, caprolactam, polyester and polyamide oligomers), polymeric additives, surfactants, and curing agents
  • Elemental impurities: lead, cadmium, mercury, arsenic, chromium, nickel, zinc, cobalt, barium, and other heavy metals aligned with ICH Q3D and regional food contact restrictions
  • High-concern substance classes: nitrosamines, primary aromatic amines, polycyclic aromatic hydrocarbons (PAHs), bisphenol A and related compounds, and per- and polyfluoroalkyl substances (PFAS)
  • General screening parameters: non-volatile residue (total extractables), pH change, ultraviolet absorbance across 200–400 nm, turbidity, and total organic carbon
  • Food contact migration items: overall migration against the 10 mg/dm² limit and specific migration against individual SML values under EU 10/2011, GB 31604, and comparable frameworks

Testing Methods

Extraction Study Design

Extraction studies apply exaggerated but justified conditions to generate a complete extractables profile. Solvent systems are selected to bracket the polarity of the intended product, typically including acidified water (pH 2–3), buffered water (pH 9–10), ethanol/water mixtures, isopropanol, and hexane or heptane for lipophilic products. Extraction is performed at defined surface-area-to-volume ratios, using controlled incubation (for example, 40 °C or 70 °C over several days), autoclave conditions (121 °C), or accelerated extraction in accordance with USP <1663> and ISO 10993-12.

Chromatographic Screening and Identification

  • Headspace GC-MS and direct-injection GC-MS (EI and CI ionization) for volatile and semi-volatile organics
  • LC-MS using triple quadrupole and high-resolution mass spectrometry (QTOF and Orbitrap platforms) for non-volatile and thermally labile organics
  • GC-FID and HPLC-UV for routine quantitative screening of target compounds
  • Size exclusion chromatography (GPC/SEC) for polymeric and oligomeric extractables

Elemental and Inorganic Analysis

  • ICP-MS and ICP-OES for multi-element quantification at trace levels
  • Ion chromatography for inorganic anions and cations, including fluoride, chloride, bromide, and sulfate

Structural Confirmation

Unknown compounds above the AET are identified through accurate-mass fragmentation, isotope pattern analysis, comparison with curated mass spectral libraries, and confirmation against authentic reference standards where available. Fourier-transform infrared spectroscopy (FTIR) and nuclear magnetic resonance spectroscopy (NMR) provide complementary structural evidence for unknowns.

Simulation and Migration Studies

Where direct product analysis is impractical, simulation studies use a simulating solvent under intended-use conditions, followed by a migration (leachables) study on actual product stored through the claimed shelf life. Leachables sampling is typically integrated into the stability program at defined time points and storage temperatures.

Method Validation and Data Interpretation

Validated quantitative leachables methods must demonstrate specificity, linearity, accuracy, precision, limit of detection, limit of quantitation, and robustness. Reported concentrations are compared with the AET, and any compound exceeding the threshold is escalated for toxicological risk assessment in accordance with ISO 10993-17, ICH Q3E principles, and recognized dose-based safety thresholds.

Applications

Extractables and leachables testing analysis supports a wide range of regulatory, quality, and development objectives:

  • Regulatory submissions for pharmaceuticals, including IND, NDA, ANDA, BLA, and DMF filings where packaging-product compatibility must be demonstrated
  • Biocompatibility documentation for medical device registration under ISO 10993-1 chemical characterization requirements in major global markets
  • Food contact material compliance with EU 10/2011, FDA 21 CFR provisions, GB 4806 series, and related national regulations
  • Submissions for electronic nicotine delivery systems and e-liquids under regional tobacco and notification frameworks
  • Material selection, supplier qualification, and change control for packaging and single-use systems
  • Root cause investigation of contamination, discoloration, odor, particulates, or adsorption interactions between product and packaging
  • Support for extractables data sharing between suppliers and drug product manufacturers under standardized protocols

Accredited third-party laboratories routinely perform these studies under ISO/IEC 17025 quality systems, providing the independent data packages required by regulators worldwide.

FAQ

What is the difference between extractables and leachables?

Extractables are compounds forced out of a material under exaggerated laboratory conditions (strong solvents, high temperature, long duration), representing a worst-case chemical profile. Leachables are compounds that actually migrate into the product under normal manufacturing, storage, and use conditions. Extractables data are used to predict and design leachables studies.

What is the Analytical Evaluation Threshold (AET)?

The AET is the concentration in a sample below which an extractable or leachable is considered too low to present a safety concern. It is calculated from the Safety Concern Threshold (typically 1.5 µg/day), the patient’s daily exposure to the product, and an analytical uncertainty factor of up to 50%, as described in USP <1663>.

How long does a complete E&L study take?

A typical extractables screening and characterization study takes 6 to 10 weeks, while a full leachables program spanning the product shelf life may run from several months to the entire stability period. Toxicological assessment adds an additional two to four weeks depending on the complexity of findings.

Which solvents and extraction conditions are used?

Solvents are chosen to bracket product polarity, commonly including water at low and high pH, ethanol/water mixtures, isopropanol, and hydrocarbons. Conditions range from controlled incubation at 40–70 °C to autoclave extraction at 121 °C, selected according to USP <1663>, ISO 10993-12, or the intended use scenario.

Why is toxicological risk assessment needed?

Identification and quantification alone do not establish safety. Compounds detected above the AET are evaluated against dose-based thresholds, structural alerts (such as nitrosamines or PAHs), and exposure calculations to determine whether patient or consumer risk is acceptable, as required by ISO 10993-17 and emerging ICH Q3E expectations.

Do food contact and pharmaceutical E&L studies differ?

Yes. Food contact testing emphasizes overall and specific migration limits under defined food simulants, times, and temperatures (EU 10/2011, GB 31604, EN 1186). Pharmaceutical E&L studies emphasize extractables profiling, AET-based reporting, validated leachables methods, and toxicological evaluation aligned with USP and ICH frameworks.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing